Gate design is one of the most consequential decisions in injection mold engineering. The gate is the smallest cross-section in the melt delivery system, yet it controls how molten plastic enters the cavity, how the part fills, and ultimately whether the part meets dimensional and cosmetic specifications. A poorly designed gate can ruin an otherwise sound mold design, while a correctly designed gate produces consistent, high-quality parts cycle after cycle.
This guide covers gate function, gate types, selection criteria, placement strategies, sizing calculations, and quality implications based on hands-on experience with production molds across a wide range of materials and applications.
What Is a Gate in Injection Molding?
A gate is the restricted opening between the runner system and the mold cavity. Its primary functions are:
- To allow molten polymer to enter the cavity at a controlled flow rate
- To freeze off quickly after cavity fill, preventing backflow of material from the cavity into the runner system
- To provide a clean break point between the runner and the finished part during ejection or secondary operations
The gate cross-section is deliberately smaller than the runner to facilitate rapid solidification at the gate seal point. This gate freeze-off timing is critical — freeze too early and the part short-fills; freeze too late and packing pressure is lost, leading to sink marks and excessive shrinkage.
At Shinzoft’s injection molding service, gate design is always reviewed during the mold design phase, because changing a gate location or size after steel is cut is expensive and time-consuming.

Types of Gates in Injection Molding
Each gate type has specific advantages, limitations, and recommended applications. The choice depends on part geometry, material rheology, production volume, and cosmetic requirements.
1. Edge Gate (Rectangular Gate)
The edge gate is the most common gate type. It is located on the parting line along the edge of the part, typically with a rectangular cross-section. Gate dimensions generally range from 0.5 to 3.0 mm in depth (usually 50-80% of the nominal wall thickness) and 1.0 to 10.0 mm in width.
Best for: Two-plate molds, flat parts, large parts requiring good flow. Works well with most thermoplastics including ABS, polycarbonate, and nylon.
Limitations: Leaves a visible gate vestige that requires manual trimming or degating. Not suitable for cosmetically critical surfaces where the gate scar is unacceptable.
2. Pin Gate (Point Gate)
A pin gate is a small circular opening, typically 0.3 to 1.5 mm in diameter. It restricts flow significantly, which generates shear heat that can lower the viscosity of shear-sensitive materials. Pin gates are commonly used in three-plate molds where the runner system is on a separate plate from the cavities.
Best for: Small to medium parts, multi-cavity molds, parts where automatic degating is desired. Works particularly well with polypropylene, polyethylene, and nylon.
Limitations: High pressure drop due to restricted flow. Not suitable for high-viscosity materials or glass-filled grades where the small gate can cause excessive shear and material degradation.
3. Submarine Gate (Tunnel Gate)
A submarine gate is located below the parting line surface and tunnels through the mold steel to the cavity. During ejection, the gate shears off automatically as the part and runner are pushed out of the mold. The gate diameter typically ranges from 0.5 to 2.0 mm.
Best for: Automatic degating applications, high-volume production, two-plate molds where no secondary degating operation is desired.
Limitations: Requires sufficient draft angle in the tunnel section. Harder to machine than edge gates. The tunnel can wear over time, especially with glass-filled materials.
4. Fan Gate
The fan gate spreads the melt across a wider entrance to the cavity, with a gradually expanding cross-section. The gate width can range from 6 to 25 mm or more, with a depth of 0.25 to 1.5 mm at the cavity entrance.
Best for: Large flat parts such as housings, panels, and covers where uniform flow across a wide front is critical. Also used for parts requiring minimal warpage.
Limitations: Leaves a relatively large gate vestige that must be machined or hand-finished. Higher tooling cost due to more complex machining.
5. Diaphragm Gate
A diaphragm gate distributes melt around the entire circumference of a cylindrical opening. It is essentially a thin disc-shaped gate around the core. Typical gate thicknesses range from 0.3 to 0.8 mm.
Best for: Cylindrical parts, tubular components, bushings. Eliminates weld lines that would form with a single edge gate on round parts.
Limitations: Requires a secondary operation to remove the diaphragm. Higher material waste in the gate area.
6. Ring Gate
Similar to the diaphragm gate but used for hollow cylindrical parts where the core is extended. The ring gate allows melt to flow around the entire core circumference. Gate thickness is typically 0.5 to 1.5 mm.
Best for: Long hollow parts, pipe fittings, cylindrical parts with a core.
Limitations: Complex machining, difficult gate removal, longer cycle time due to gate cooling.
7. Sprue Gate
The sprue gate feeds the cavity directly from the sprue bushing — the part attaches directly to the sprue with no runner. The gate dimension essentially matches the sprue O-diameter at the cavity entrance, typically 3 to 8 mm.
Best for: Single-cavity molds, large parts, prototype molds, low-volume production. Ideal for materials sensitive to shear heating since the large opening minimizes pressure drop.
Limitations: Leaves a large gate scar that requires sawing or machining to remove. No runner system, which simplifies the mold but limits cavity count.
8. Tab Gate
The tab gate incorporates a small tab or land between the runner and the cavity. This tab acts as a shear zone where melt energy is dissipated before entering the cavity. The tab is usually 0.5 to 2.0 mm thick and 3.0 to 10.0 mm wide.
Best for: Parts where jetting is a concern, flexible materials, decorative parts requiring minimal gate blush.
Limitations: Additional material consumption in the tab area. The tab requires trimming in a secondary operation.
9. Hot Tip Gate (Hot Runner Gate)
Used exclusively in hot runner systems, the hot tip gate sits directly at the cavity entrance with the nozzle maintained at melt temperature. Gate diameters range from 0.5 to 2.5 mm depending on the hot drop manufacturer and material being processed.
Best for: High-volume production, multi-cavity and family molds, parts requiring no runner waste. Compatible with most engineering thermoplastics.
Limitations: Higher initial mold cost due to hot runner system expense. Requires more maintenance. Thermal control is critical — a frozen nozzle causes downtime.
Gate Selection Criteria
Choosing the right gate type requires evaluating these factors in order of priority:
Part Geometry
Wall thickness, part volume, and overall geometry dictate gate placement and type. Thin-wall parts (< 1.0 mm) typically require larger gates to fill before freeze-off. Thick sections benefit from gates positioned to favor packing.
Material Selection
Each resin behaves differently at the gate. For example, glass-filled nylons (PA6-GF30 or PA66-GF30) are abrasive and cause accelerated gate wear, so hardened steel gate inserts are recommended. Polycarbonate has high melt viscosity and requires a generously sized gate to prevent shear burning — a 0.8 mm minimum gate depth is a good starting rule for PC. Liquid silicone rubber (LSR) requires a different gate philosophy altogether, typically using cold deck technology with pinpoint gates.
Refer to Shinzoft’s material guide for detailed processing parameters and gate recommendations per resin family.
Production Volume
High-volume production (> 500,000 parts/year) justifies hot runner systems with hot tip gates due to automatic operation and zero runner waste. Low-volume runs (< 10,000 parts) are better suited to simple two-plate molds with edge or submarine gates.
Cosmetic Requirements
Parts with Class A surfaces require gate locations that leave no visible vestige. Pin gates with three-plate molds or hot tip gates are preferred. Submarine gates can work if the vestige is in a non-critical area.
Gate Placement Principles
Gate location is equally important as gate type. Poor gate placement causes flow imbalance, weld lines, air traps, and cosmetic defects. These are the engineering principles we apply at Shinzoft’s mold manufacturing service:
Flow Balance
The gate should be positioned to achieve balanced flow — meaning the melt front reaches all extremities of the cavity simultaneously. In multi-cavity molds, flow balance across cavities is non-negotiable. Imbalanced fill causes variations in packing, shrinkage, and part dimensions.
Weld Line Management
Weld lines form where two melt fronts meet. Gates should be placed to minimize weld lines in structurally critical areas. When weld lines are unavoidable, position gates to push weld lines to low-stress regions or ensure they merge at high enough temperature to maintain adequate knit-line strength. For glass-reinforced materials, weld line strength can be as low as 30-50% of the bulk material strength.
Air Trap Prevention
Gate placement determines the air venting path. The last-filled areas should align with mold vents. If the gate position forces air to be trapped at a weld line or in a dead-end pocket, the result is burn marks, short shots, or incomplete weld line fusion.
Aesthetic Surface Consideration
Gate placement should avoid visible surfaces. In cosmetic parts, the gate should be located on the inside, the underside, or surfaces that will be hidden in the final assembly. Gating directly into a textured surface is generally avoided because the flow pattern creates visible gate blush or flow marks.
Gate Size Calculation Guidelines
Gate sizing starts from the nominal wall thickness of the part. These are practical starting points:
| Wall Thickness (mm) | Gate Depth (mm) | Gate Width (mm) | Typical Gate Type |
|---|---|---|---|
| 0.5 – 1.0 | 0.3 – 0.5 | 1.0 – 3.0 | Pin gate, submarine gate |
| 1.0 – 2.0 | 0.5 – 1.2 | 2.0 – 6.0 | Edge gate, tab gate |
| 2.0 – 3.0 | 1.2 – 2.0 | 4.0 – 10.0 | Edge gate, fan gate |
| 3.0 – 5.0 | 2.0 – 3.0 | 6.0 – 15.0 | Fan gate, sprue gate |
The gate depth should generally not exceed 80% of the nominal wall thickness to ensure clean gate freeze-off. Gate width is typically 2 to 5 times the gate depth for edge gates. For pin gates, the diameter should be 50-80% of the wall thickness.
A useful rule of thumb: the gate cross-sectional area should be approximately 5-10% of the runner cross-sectional area. This ensures the gate freezes before the runner, preventing backflow from the cavity.
Gate Design and Part Quality
Sink Marks
Sink marks occur when the gate freezes before the thick sections have fully packed out. Increasing gate size, relocating the gate closer to the thick section, or extending hold time can help. In polypropylene or polyethylene parts, delayed gate freeze using a larger gate is often the fix.
Jetting
Jetting happens when melt shoots through the gate without contacting the cavity walls, forming a wavy or worm-like pattern. This is common when gating into thin sections that lead to thicker sections. Solutions include: increasing gate size, using a tab gate, modifying gate location to direct flow against a core or wall, or reducing injection speed through the gate area.
Flow Marks
Flow marks (gate blush) appear as rings or streaks around the gate area. They are caused by the melt cooling as it expands into the cavity, combined with hesitation or pressure drops. Higher melt temperature, larger gate cross-section, and increased injection speed reduce flow marks.
Gate Vestige
The gate vestige is the mark left after the gate is separated from the part. Acceptable vestige height depends on the application. For consumer products, less than 0.05 mm protrusion is typical. For industrial parts, 0.1 to 0.2 mm may be acceptable. Submarine gates naturally shear flush during ejection. Hot tip gates leave a small nub that can be controlled by gate diameter and gate cooling design.
Gate Design Review Checklist
- Gate type matches material rheology and volume requirements
- Gate location provides balanced cavity fill (validated by mold flow analysis)
- Gate size allows adequate packing without premature freeze-off
- Gate vestige is acceptable for the application
- Gate design is compatible with the runner system (see our guide on runner system design)
- Gate area is accessible for machining and polishing
- Ejection system does not interfere with gate location
Conclusion
Gate design is a balancing act between filling, packing, aesthetics, and economics. The right gate produces consistent, defect-free parts. The wrong gate creates headaches in processing, quality, and secondary operations. By understanding gate types, applying placement principles, and sizing correctly, mold designers can significantly reduce first-shot iterations and production downtime.
Frequently Asked Questions
What is the most common gate type in injection molding?
The edge gate is the most widely used gate type due to its simplicity, ease of machining, and compatibility with a broad range of part geometries and materials.
How do I choose between a cold runner submarine gate and a hot tip gate?
Submarine gates are economical for cold runner molds in medium-volume production and provide automatic degating. Hot tip gates are preferred for high-volume production where zero runner waste and faster cycles justify the higher tooling investment.
What gate type is best for glass-filled materials?
Edge gates or fan gates with hardened inserts are recommended for glass-filled materials. Small pin gates should be avoided because the abrasive glass fibers cause rapid gate wear and inconsistent fill.
Can I relocate a gate after the mold is built?
Relocating a gate after mold construction requires welding the existing gate opening, re-machining the cavity steel, and re-texturing if applicable. It is possible but costly. This is why thorough mold flow analysis before steel cutting is strongly recommended.
What gate vestige height is acceptable for consumer products?
For consumer-facing surfaces, gate vestige should be less than 0.05 mm. For non-visible surfaces, 0.1 to 0.2 mm is typically acceptable. Submarine and hot tip gates are preferred when minimal vestige is required.
Need expert assistance with your injection mold project? Contact Shinzoft for professional mold design and manufacturing services.
— Article by Shinzoft Engineering Team