Polypropylene (PP) is the lightest general-purpose plastic at 0.90–0.91 g/cm³, combining outstanding fatigue resistance with broad chemical resistance and a melting point of 160–170 °C. It is the standard material for living hinges, automotive trim, medical devices, food containers, and battery housings. Shinzoft provides OEM/ODM PP injection molding from DFM and tooling through validated mass production.
At 0.90–0.91 g/cm³, PP is lighter than PE, PS, and ABS. That translates into fewer grams per part and better cost-performance in high-volume production.
PP homopolymer withstands repeated flexing better than almost any other thermoplastic. A correctly designed hinge can survive tens of thousands of open-close cycles without cracking.
Resistant to acids, alkalis, salts, alcohols, and most detergents. PP handles aggressive cleaning agents and many solvents that would attack PS or ABS.
Melting point of 160–170 °C and an HDT around 90–105 °C at 0.45 MPa let PP parts go where PE cannot, including dishwasher-safe and hot-fill applications.
These values cover unfilled, general-purpose grades. Homopolymer, random copolymer, and impact copolymer differ meaningfully, so treat the ranges as a guide and confirm against the grade you select.
| Property | Typical Value | Notes |
|---|---|---|
| Density | 0.90–0.91 g/cm³ | Lightest of the common commodity plastics |
| Tensile Strength (Yield) | 25–40 MPa | Homopolymer at the high end, copolymer lower |
| Flexural Modulus | 1,100–1,600 MPa | Good stiffness for a low-density material |
| HDT at 0.45 MPa | 90–105 °C | Suitable for hot-fill and dishwasher cycles |
| Melting Point | 160–170 °C | Higher than any polyethylene grade |
| Molding Shrinkage | 1.2–2.5 % | Higher with impact copolymer and thick walls |
| Water Absorption | <0.02 % | Essentially non-hygroscopic, no drying needed |
| Notched Izod Impact (23 °C) | 20–80 J/m | Homopolymer is notch-sensitive; copolymers improve toughness |
| Dielectric Strength | 20–28 kV/mm | Good insulation for appliance and electrical parts |
| Parameter | Typical Range |
|---|---|
| Drying Temperature / Time | Not required (non-hygroscopic; keep pellets clean and dry) |
| Melt Temperature | 200–260 °C |
| Mold Temperature | 20–60 °C |
| Injection Pressure | 60–120 MPa |
| Holding Pressure | 40–80 MPa |
| Typical Cycle Time | 20–50 s (depends on wall thickness) |
PP is a high-shrinkage, high-crystallinity material, so mold temperature drives both shrinkage and surface quality. Running the mold hotter improves gloss and weld-line strength but increases shrinkage, so the setting must be locked in early and applied consistently. For living hinges, gate orientation is critical: the melt must flow across the hinge line to align polymer chains, and the hinge should be filled quickly before it freezes. PP is notch-sensitive, so avoid sharp corners in the part design.
Against the PE family, PP is lighter, stiffer at temperature, and far superior in living hinges and fatigue life, while PE wins on low-temperature impact and toughness. Compared with PE-PP blends, straight PP offers the highest stiffness and best hinge performance, whereas a blend trades some rigidity for flexibility, better stress crack resistance, and lower cost. Against TPE, PP is rigid and structural while TPE provides rubber-like softness and grip, so the two are often combined in overmolded two-shot parts where a hard PP substrate meets a soft TPE skin.
Choose homopolymer for maximum stiffness, heat resistance, and living hinge performance. Choose random copolymer when clarity and better low-temperature toughness matter. Choose impact copolymer when you need the best drop impact, especially below room temperature, and can accept slightly lower stiffness and higher shrinkage.
Three things matter most: thin the hinge to roughly 0.25–0.5 mm, gate the part so the melt flows across the hinge line to align the polymer chains, and radius both faces of the flex zone. Never let a weld line or gate mark land in the hinge, and use homopolymer PP for the highest cycle life.
Expect 1.2–2.5%, with impact copolymer and thick walls at the higher end. Keep wall thickness uniform, balance the runner so all cavities fill evenly, and cool both halves of the tool symmetrically. In glass-filled grades, gate position also controls fiber orientation, which strongly affects distortion.
Yes, with the correct grade. Food-contact compliant and medical-grade PP are widely available, and PP handles hot filling and dishwasher temperatures better than PE or PS. Tell us the regulatory requirement at the start of the project so we can specify and document the compliant resin from the outset.
No. PP is non-hygroscopic with water absorption below 0.02%, so drying is not part of the standard process. For glass-filled or specialty grades, check the supplier's recommendation, since fillers and additives can change moisture behavior. Otherwise, simply keep the pellets clean and free of surface condensation.
Send us your drawings and get a quote with a free DFM analysis covering hinge design, gate placement, and warpage control.
Shinzoft serves customers worldwide with custom PP injection molding solutions, and you can review other polymers on our materials page.
Get a Free Quote →