POM (Acetal/Delrin) Injection Molding Material Supplier & Manufacturer

Polyoxymethylene (POM), also known as Acetal or Delrin, is a semi-crystalline engineering thermoplastic known for its low friction, outstanding wear resistance, high stiffness, and dimensional stability in humid conditions. It replaces metal in precision gears, bearings, bushings, snap-fits, zippers, and fuel-system parts. Shinzoft delivers OEM/ODM POM injection molding from DFM and tooling through validated mass production.

Key Properties of POM for Injection Molding

Low Friction & Wear

The lowest coefficient of friction of any unfilled engineering plastic, roughly 0.15–0.35 against steel. Parts run dry without lubrication, ideal for gears, bushings, and sliding assemblies.

High Stiffness & Fatigue Life

Tensile strength of 60–70 MPa and flexural modulus near 2,600–3,100 MPa give POM metal-like rigidity. It survives millions of stress cycles without cracking.

Dimensional Stability

Moisture absorption of only 0.2–0.3% keeps molded dimensions steady through humidity changes, so tight tolerances hold far better than with hygroscopic materials.

Chemical & Fuel Resistance

Good resistance to fuels, oils, greases, and mild solvents, with copolymer grades also handling hot water and alkalis. Ideal for automotive fluid handling.

Technical Specifications of POM

Typical values below refer to unfilled general-purpose grades. Specific figures vary with grade, supplier, and homopolymer versus copolymer formulation.

PropertyTypical ValueNotes
Density1.41 g/cm³Higher than ABS or nylon; slightly higher for homopolymer
Tensile Strength60–70 MPaMetal-replacement stiffness at room temperature
Flexural Modulus2,600–3,100 MPaStiff, rigid parts with little creep
Heat Deflection Temp (HDT, 1.8 MPa)95–110 °CCopolymer grades favor the upper end
Melting Point165–175 °CSharp melting transition of a highly crystalline polymer
Molding Shrinkage1.8–2.5 %High and directional; mold compensation is essential
Dielectric Strength18–20 kV/mmGood electrical insulation for switch and connector parts

Applications of POM Injection Molding

  • ✅ Precision Motion Parts: gears, racks, cams, pulleys, worm wheels, and bearing cages that run on metal shafts
  • ✅ Bearings & Bushings: sleeve bearings, thrust washers, and slider blocks for dry-running assemblies
  • ✅ Automotive & Fuel Systems: fuel caps, pump and valve housings, window-lifter gears, seat adjusters, and pneumatic valve bodies
  • ✅ Fasteners & Hardware: snap-fits, clips, buckles, hinges, and zipper components
  • ✅ Industrial & Appliances: metering components, conveyor parts, switch mechanisms, and actuator housings

POM Injection Molding Process Parameters

ParameterTypical Range
Drying Temperature / TimeUsually not required; if moisture > 0.2%, 80 °C / 2–4 h
Melt Temperature190–230 °C (copolymer 190–220 °C, homopolymer 200–230 °C)
Mold Temperature60–100 °C
Injection Pressure70–120 MPa
Typical Cycle Time20–60 s, depending on wall thickness

Two process notes matter most. POM degrades quickly when overheated and can release formaldehyde, so hold barrel temperatures within grade limits and keep residence time short — a blocked nozzle or stalled cycle is enough to scorch the melt. Also, never let POM share a machine or regrind stream with PVC, as the two decompose violently together. Fast crystallization means short cycles, but thick sections still need generous packing to offset shrinkage.

Design & Tooling Considerations for POM

  • Shrinkage compensation: at 1.8–2.5% POM shrinks far more than ABS or PC. Size the mold cavities accordingly and keep wall thickness uniform so different areas do not pull at different rates.
  • Warpage control: balance the gate layout, use adequate hold pressure, and avoid abrupt thickness changes. Voids form in heavy sections when the core cools faster than the skin.
  • Gating and venting: use generous runners with smooth transitions; add vents at the last-fill locations to prevent burn marks. Sharp gates shear the melt and create weak weld lines.
  • Radii and ribs: generous fillets reduce molded-in stress; ribs add stiffness without the sinking that a thick wall would cause.
  • Tool steel selection: POM releases acidic byproducts during a thermal excursion, so corrosion-resistant steels and a clean, well-polished surface extend tool life and part quality.

POM vs Other Injection Molding Materials

POM and Nylon (PA) are the two workhorses of dry-running mechanical parts, but they behave differently. Nylon is tougher and more fatigue-resistant but absorbs 2.5–3% moisture, so its dimensions and stiffness shift as it takes on water; POM holds its shape and its friction characteristics stay flat. Where a part must run quietly and hold tolerance without lubrication, POM usually wins.

Against PBT, POM offers lower friction and better toughness, while PBT handles higher continuous temperatures and holds tighter electrical tolerances. For chemical and water exposure, POM copolymer beats most Polyethylene (PE) grades in stiffness and load capacity, though PE remains the cheaper choice for non-structural parts.

Related Injection Molding Materials

Why Choose Our Factory for POM Injection Molding

  • ISO 9001 Certified Quality: documented process control, in-process SPC on critical gear dimensions, and PPAP documentation for automotive programs.
  • 15+ Years of Experience: founded in 2010 in Shenzhen, with 50+ molding machines and a Huizhou plant producing more than 30 million parts for over 1,000 customers.
  • Free DFM Analysis: we review wall thickness, shrinkage compensation, gate location, and gear geometry before cutting steel, with no minimum order quantity.
  • Fast Lead Time: most orders ship within 15 working days, backed by multi-cavity tooling and automation for gear and bushing volumes.

FAQs About POM Injection Molding

Should I choose homopolymer or copolymer POM?

Homopolymer POM is about 10–15% stiffer and stronger, so it suits high-load gears and structural parts. Copolymer POM has better resistance to hot water, steam, and alkaline chemicals and a slightly wider processing window, making it the better choice for plumbing, medical, and fuel-system components.

Do POM gears and bearings need lubrication?

POM has a low coefficient of friction and good self-lubricating behavior, so many gears and bushings run dry. For high loads or fast surface speeds, a light grease or a PTFE-filled grade reduces heat and extends service life. We size the part for the intended lubrication state during DFM.

How do I deal with POM's high shrinkage rate?

POM shrinks 1.8–2.5%, so the mold must be cut oversize based on the actual grade data sheet, not a generic figure. Uniform wall thickness, balanced gating, sufficient holding pressure, and generous cooling all keep shrinkage even across the part and prevent voids in thick sections.

Can POM be used outdoors or in humid environments?

POM absorbs very little water — around 0.2–0.3% — so it holds dimensions in humid air and even in immersion. UV exposure degrades the surface over time, so outdoor parts should use a UV-stabilized grade, often carbon-black filled, and be designed to avoid long-term direct sunlight where possible.

What are the main processing precautions for POM?

Keep melt temperature within grade limits because overheating releases formaldehyde and burns the melt; shorten residence time and purge thoroughly during shutdowns. Never run POM on equipment previously used for PVC without full purging, as the combination can decompose rapidly. Proper venting also prevents burn marks at the last-fill points.

Looking for a Reliable POM Injection Molding Partner?

Send your drawings, target tolerances, load and tribology requirements, and compliance needs. Our engineers will recommend the right POM grade and deliver stable, repeatable production.

Shinzoft serves customers worldwide with custom POM injection molding solutions and a full range of injection molding materials.

Get a Free Quote →
TYPE TO SEARCH

Tel:+86 0752-3336216
Email:Sales@shinzoft.com