PETG (glycol-modified PET) is a clear amorphous copolyester that delivers glass-like transparency, better toughness than PMMA and standard PET, and far easier processing with lighter drying demands. It resists many chemicals, meets food-contact requirements, and tolerates radiation sterilization. It is used for transparent guards, medical devices such as test tube racks and culture boxes, cosmetic packaging, display signage, and 3D printing filament. Shinzoft runs OEM/ODM PETG injection molding from DFM and tooling through validated mass production.
PETG transmits close to 90% of visible light with low haze, yet resists impact far better than PMMA or standard PET. Clear parts survive dropping and handling instead of cracking, which is why it replaces acrylic in many protective and display uses.
PETG is far more forgiving than PC or PET. Drying is lighter — around 65–70 °C for 4 hours — and it flows readily at moderate temperatures, which shortens setup and reduces rejects on startup.
PETG withstands many household chemicals, alcohols, and cleaning agents that craze acrylic. It also resists stress cracking better than PS, so transparent parts stay clear through normal use and cleaning.
Food-contact grades are readily available, and PETG accepts gamma and e-beam radiation sterilization without yellowing or losing strength — a practical advantage for medical trays, racks, and packaging.
Values reflect general-purpose unfilled PETG copolyester; clarity, ductility, and low shrinkage are its defining characteristics.
| Property | Typical Value | Notes |
|---|---|---|
| Density | 1.27–1.33 g/cm³ | Unfilled amorphous grade |
| Tensile Strength | 50–55 MPa | Ductile, high elongation |
| Flexural Modulus | 2,000–2,300 MPa | Less stiff than PET, more ductile |
| Notched Izod Impact | 60–100 J/m | Tougher than PMMA and PET |
| Heat Deflection Temp (HDT, 1.8 MPa) | 65–75 °C | Lower than PC or PET |
| Melting Point / Tg | Amorphous / ~80 °C | No sharp melting point |
| Molding Shrinkage | 0.2–0.6 % | Low and uniform |
| Dielectric Strength | 15–20 kV/mm | Good insulation |
| Light Transmission | Up to 90 % | Clear grade |
| Parameter | Typical Range |
|---|---|
| Drying Temperature / Time | 65–70 °C / 4 h (lighter than PC or PET) |
| Melt Temperature | 230–260 °C |
| Mold Temperature | 20–50 °C |
| Injection Pressure | 50–90 MPa |
| Typical Cycle Time | 20–45 s (wall-thickness dependent) |
PETG is one of the easier transparent resins to mold, but a few rules matter. Dry at 65–70 °C for about four hours to avoid splay on clear surfaces. Keep melt temperature within 230–260 °C; overheating degrades the copolyester and causes yellowing. Cool molds of 20–50 °C give short cycles and good clarity. Because PETG stays amorphous on cooling, it does not need the high mold temperatures that PET requires, and can often be run in standard water-cooled tooling.
Compared with standard PET, PETG trades crystallinity for clarity and toughness: it is easier to process and far more ductile, though less stiff and less heat resistant. Against PC, PETG is less impact resistant and has a much lower heat deflection temperature, but it costs less, molds more easily, and resists some chemicals that attack PC. Compared with PMMA (Acrylic), PETG is slightly less clear but dramatically tougher and more forgiving to process, making it the better choice for parts that get handled.
PETG adds a glycol modifier that prevents crystallization, so it stays amorphous, clear, and ductile instead of turning opaque and rigid. That makes PETG far easier to mold, more impact resistant, and better suited to transparent parts. Standard PET is stiffer, harder, and more heat resistant, which suits wear parts and precision components.
Yes, but far less aggressively than PC or PET. Dry PETG at 65–70 °C for about four hours to remove surface moisture that causes splay on clear parts. Because it does not hydrolyze as severely as PET, the drying window is more forgiving, which helps shorten setup time on new jobs.
Yes. Food-contact PETG grades are widely available, and PETG accepts gamma and e-beam radiation sterilization without yellowing or losing strength, which suits test tube racks, culture boxes, trays, and packaging. Specify a compliant grade and confirm the sterilization method with your supplier before production.
For parts that get handled or dropped, yes. PETG is markedly tougher than PMMA and resists the crazing and cracking that acrylic suffers under stress and chemical contact. Acrylic still wins on ultimate clarity and UV stability, so choose PMMA for display optics and PETG for guards, covers, and any clear part exposed to impact.
PETG reaches an HDT of roughly 65–75 °C at 1.8 MPa, which is lower than PC or PET because the material stays amorphous. It handles warm indoor conditions and normal consumer use well but should not be specified for parts that see sustained high heat or hot-fill conditions. For higher heat, PET, PC, or a PC alloy is the better route.
Send us your drawings and requirements — clarity, sterilization method, food contact — and we will match the right PETG grade, quote it, and support it with a free DFM analysis.
Shinzoft serves customers worldwide with custom PETG injection molding solutions from prototype to mass production. Explore the full range on our materials page.
Get a Free Quote →