PET Injection Molding Supplier & Manufacturer

PET (polyethylene terephthalate) is a semi-crystalline engineering polyester with high surface hardness, good wear resistance, and excellent dimensional stability. Reinforced with glass fiber it becomes genuinely rigid — a flexural modulus above 9,000 MPa — while holding tight tolerances. It is used for electrical connectors, automotive electrical parts, gears, bearing cages, and food-grade containers. Shinzoft delivers OEM/ODM engineering PET injection molding from DFM and tooling through validated mass production.

Key Properties of PET for Injection Molding

Surface Hardness & Wear

PET has one of the harder surfaces among common engineering thermoplastics, which resists scratching and abrasion in moving or handled parts. That hardness, paired with low friction, suits gears, cams, and sliding components.

High Stiffness When Filled

Unfilled PET is already stiff; adding 30% glass fiber lifts flexural modulus past 9,000 MPa, letting thin sections carry loads that would need much thicker walls in an unfilled resin.

Dimensional Stability

Low moisture uptake and a crystalline structure keep PET parts dimensionally predictable. Glass-filled grades shrink only 0.2–0.5%, enabling the tight tolerances electrical connectors demand.

Chemical & Heat Resistance

PET resists oils, greases, and many solvents, and it holds an HDT of about 80 °C unfilled — rising past 200 °C with glass fill and heat stabilization. It is also widely approved for food-contact applications.

Technical Specifications of PET

Values below cover general-purpose unfilled PET; glass-filled engineering grades are far stiffer and more heat resistant.

PropertyTypical ValueNotes
Density1.33–1.40 g/cm³Unfilled crystalline grade
Tensile Strength55–75 MPa30% GF reaches 140–160 MPa
Flexural Modulus2,400–3,100 MPa30% GF exceeds 9,000 MPa
Notched Izod Impact20–40 J/mNotch sensitive, lower when GF
Heat Deflection Temp (HDT, 1.8 MPa)~80 °CGF and heat-stabilized grades reach 200 °C+
Melting Point / Tg~250–260 °C / 70–80 °CSemi-crystalline polyester
Molding Shrinkage1.0–2.0 %0.2–0.5% with 30% GF
Dielectric Strength15–20 kV/mmGood insulation for electrical parts
Water Absorption (24 h)0.1–0.3 %Low, supports dimensional stability

Applications of PET Injection Molding

  • ✅ Electrical Connectors: plugs, sockets, terminal blocks, coil formers, precision sockets requiring tight tolerances
  • ✅ Automotive Electrical Parts: sensor housings, ignition components, switch bodies, lamp sockets
  • ✅ Gears & Mechanical Parts: spur and helical gears, cams, bushings, wear pads, sliding components
  • ✅ Bearing Cages: roller and ball bearing retainers, thrust washers, guide rings
  • ✅ Food-Grade Containers: food-contact trays, closures, and packaging components in approved grades
  • ✅ Appliance & Industrial: pump housings, valve parts, housings, textile machinery components

PET Injection Molding Process Parameters

ParameterTypical Range
Drying Temperature / Time150 °C / 4 h or more (mandatory)
Melt Temperature270–300 °C
Mold Temperature80–120 °C (higher for crystallinity)
Injection Pressure70–110 MPa
Typical Cycle Time25–60 s (wall-thickness dependent)

PET demands thorough drying: 150 °C for at least four hours with a dew-point dryer, since any residual moisture hydrolyzes the melt and drops intrinsic viscosity — the material literally loses strength and becomes brittle. Keep the melt in the 270–300 °C window and help crystallization with a warm mold of 80–120 °C. A cold mold produces an under-crystallized, brittle part; a properly heated one produces strong, dimensionally stable parts with consistent surface hardness.

Design & Tooling Considerations for PET

  • Shrinkage planning: unfilled PET shrinks about 1.0–2.0%; with 30% glass fill it drops to 0.2–0.5% but becomes directional. Design with grade-specific data and keep walls uniform.
  • Dry rigorously: specify 150 °C / 4 h+ with a dew-point dryer and verify moisture below 0.02%. Insufficient drying is the leading cause of brittle PET parts.
  • Warm molds: use 80–120 °C mold temperature to develop crystallinity; cold tools yield weak, cloudy parts that fail in service.
  • Notch sensitivity: PET has low notched impact, so use generous radii, avoid sharp steps, and use adequate gate sizes to limit shear.
  • Warpage control on filled grades: balance runners and cooling so glass-filled parts shrink evenly and hold flatness.

PET vs Other Injection Molding Materials

PET and PBT share the same polyester chemistry, but PET brings higher surface hardness, stiffness, and hardness while PBT crystallizes faster for shorter cycles. Where PET needs a toughness and heat boost without losing its processing character, PC-PET alloy adds impact strength and weather resistance for housings and panels. When a part must be clear and easy to process, PETG keeps the PET backbone but swaps crystallinity for clarity and toughness.

Related Injection Molding Materials

Why Choose Our Factory for PET Injection Molding

  • ISO 9001 Certified Quality: dew-point dryers, verified moisture checks, and strict melt control protect PET's intrinsic viscosity and part strength.
  • 15+ Years of Experience: since 2010 we have produced 30M+ parts for 1,000+ customers, including precision electrical and food-grade programs.
  • Free DFM Analysis: we review shrinkage, gate sizing, and cooling before tooling, so PET parts reach full crystallinity instead of turning brittle.
  • Fast Lead Time & No MOQ: 50+ machines across Shenzhen and Huizhou, most orders shipped within 15 working days, no minimum order quantity.

FAQs About PET Injection Molding

Why is drying so critical for PET injection molding?

PET hydrolyzes when moisture meets melt temperature, breaking polymer chains and lowering intrinsic viscosity. The result is brittle, weak parts. Dry at 150 °C for four hours or more with a dew-point dryer and confirm moisture below 0.02% before processing — this single step decides whether the parts perform as designed.

Can PET be glass filled for higher stiffness?

Yes. Adding 30% glass fiber lifts flexural modulus above 9,000 MPa and heat deflection temperature past 200 °C when the grade is heat stabilized. Glass-filled PET is common in connectors, gears, and structural electrical parts. Expect lower impact strength and directional shrinkage, which call for balanced gate and cooling design.

What is the difference between PET and PBT for injection molding?

Both are polyesters, but PET offers higher surface hardness, stiffness, and hardness retention, while PBT crystallizes faster and is easier to flame retard. PET suits wear parts, gears, and precision electrical components; PBT fits fast-cycling connectors and housings. The choice usually comes down to whether hardness and stiffness or cycle speed and processing ease matter more.

Are PET parts food safe?

Food-contact PET grades are widely used in packaging and containers and are approved for direct food contact. To stay compliant, use a resin certified for food contact, keep processing conditions within the supplier's guidance, and avoid regrind contamination. We can source food-grade grades on request and document compliance for your program.

Why do PET parts sometimes come out cloudy or brittle?

Cloudiness and brittleness almost always point to low crystallinity, which comes from a cold mold, or to degraded molecular weight from wet resin. Raise the mold temperature to 80–120 °C, ensure the drying is complete, and keep melt temperature within 270–300 °C. Correcting these three variables restores strength and a uniform surface.

Looking for a Reliable PET Injection Molding Partner?

Send your drawings and tell us the load, temperature, and tolerance requirements — we will select the right PET grade, quote it, and back it with a free DFM analysis.

Shinzoft serves customers worldwide with custom PET injection molding solutions from prototype tooling to mass production. See the full range on our materials page.

Get a Free Quote →