PC-PBT Alloy Injection Molding Supplier & Manufacturer

PC-PBT is a thermoplastic alloy that blends the toughness and heat resistance of polycarbonate with the chemical and oil resistance of PBT. The result resists gasoline, greases, and many solvents that attack plain PC, while keeping good impact strength at low temperatures. It suits automotive bumper trim, exterior parts, fuel filler caps, power tool housings, and lawn equipment shrouds. Shinzoft provides OEM/ODM PC-PBT injection molding from DFM and tooling through validated mass production.

Key Properties of PC-PBT for Injection Molding

Chemical & Oil Resistance

The PBT phase gives the alloy real resistance to gasoline, diesel, engine oil, greases, and many cleaning solvents. This is the key gap it closes against plain PC, which stress-cracks quickly when exposed to fuels and hydrocarbons.

Impact Strength at Low Temperature

PC-PBT keeps useful notched Izod values in the 400–700 J/m range and retains ductility well below freezing, so exterior parts survive cold-weather knocks and stone strikes instead of cracking.

Heat Resistance

Heat deflection temperatures land between 110 and 130 °C at 1.8 MPa depending on the PC/PBT ratio. That covers under-hood brackets, lighting hardware, and outdoor equipment that see sustained heat and sun.

Dimensional Stability

Crystalline PBT phase and low moisture uptake combine to keep dimensions steady. Shrinkage of about 0.6–1.2% is more predictable than semi-crystalline resins alone, helping large exterior panels hold their fit.

Technical Specifications of PC-PBT

Values reflect general-purpose unfilled PC-PBT alloy grades and shift with the blend ratio, so confirm the exact grade for critical tolerances.

PropertyTypical ValueNotes
Density1.20–1.25 g/cm³Depends on PC/PBT ratio
Tensile Strength50–65 MPaBalanced ductility
Flexural Modulus2,000–2,400 MPaStiffer than unfilled PBT
Notched Izod Impact400–700 J/mHolds up at low temperature
Heat Deflection Temp (HDT, 1.8 MPa)110–130 °CHigher with more PC content
Melting Point / Tg~225 °C / 120–140 °CPBT melt, PC glass transition
Molding Shrinkage0.6–1.2 %More uniform than PBT alone
Dielectric Strength15–20 kV/mmFine for non-critical electrical use

Applications of PC-PBT Injection Molding

  • ✅ Automotive Bumper Components: bumper brackets, energy absorbers, trim clips, mounting brackets
  • ✅ Exterior Trim Parts: grille components, wheel arch liners, mirror housings, body side molding
  • ✅ Fuel System Parts: fuel filler caps, filler necks, vapor line clips, small fuel-adjacent housings
  • ✅ Power Tool Housings: drill and grinder casings, battery interface housings, tool grips
  • ✅ Lawn & Outdoor Equipment: mower shrouds, guard housings, brush cutter covers, garden tool shells
  • ✅ Industrial Enclosures: equipment covers exposed to oils, lubrication points, machine guards

PC-PBT Injection Molding Process Parameters

ParameterTypical Range
Drying Temperature / Time120 °C / 3–4 h
Melt Temperature250–280 °C
Mold Temperature60–90 °C
Injection Pressure70–120 MPa
Typical Cycle Time25–60 s (wall-thickness dependent)

Both phases are moisture sensitive, so a thorough 120 °C dry cycle is essential to avoid splay and hydrolysis of the PBT fraction. Keep melt temperatures below roughly 280 °C: excessive heat degrades the PBT phase and dulls mechanical performance. PC-PBT cools into a semi-crystalline structure, so moderate mold temperatures of 60–90 °C and balanced cooling produce the best surface finish on large exterior parts.

Design & Tooling Considerations for PC-PBT

  • Shrinkage planning: plan around 0.6–1.2% and keep walls uniform. Large panels warp when thickness varies, so add ribs instead of thickening sections.
  • Avoid sharp corners: PC-PBT is tougher than PBT but not as forgiving as pure PC. Rounded corners and generous draft reduce molded-in stress and cracking risk.
  • Gate placement: use a balanced runner layout for multi-cavity tools, and place gates where weld lines will be hidden or least loaded on structural parts.
  • Vent generously: vent the cavity to release trapped gas; poor venting shows up as burns and short shots on large, thin exterior panels.
  • Chemical contact review: while the alloy resists fuels and oils, confirm specific exposure with a resin supplier and test functional parts before production.

PC-PBT vs Other Injection Molding Materials

Compared with plain PC, the alloy trades a little clarity and some peak toughness for far better resistance to gasoline, oils, and greases — the reason it dominates fuel-adjacent and under-hood parts. Against unfilled PBT, it is notably tougher and less brittle at low temperature, though PBT wins on flow and cost where chemical resistance is the only requirement. When clarity and easier processing matter more than chemical resistance, ABS-PC alloy is often the more economical choice.

Related Injection Molding Materials

Why Choose Our Factory for PC-PBT Injection Molding

  • ISO 9001 Certified Quality: controlled drying, temperature monitoring, and RoHS/REACH-compliant material handling for every production lot.
  • 15+ Years of Experience: established in 2010, we have produced 30M+ parts for 1,000+ customers across automotive and industrial sectors.
  • Free DFM Analysis: alloy grades behave differently from single resins, so we verify shrinkage, gate location, and cooling before committing to steel.
  • Fast Lead Time & No MOQ: 50+ machines across our Shenzhen and Huizhou plants deliver most orders within 15 working days, with no minimum order quantity.

FAQs About PC-PBT Injection Molding

What is PC-PBT alloy used for?

PC-PBT is chosen wherever a part needs PC-level toughness plus resistance to fuels, oils, and greases. Typical uses include automotive bumper brackets and exterior trim, fuel filler caps, power tool housings, and lawn equipment shrouds. It is a strong fit for any part that contacts hydrocarbons or is expected to survive cold-weather impact.

Is PC-PBT better than pure PC for automotive parts?

For parts exposed to gasoline, engine oil, and greases, yes. Plain PC stress-cracks on contact with many hydrocarbons, while PC-PBT resists them. Pure PC remains clearer and slightly tougher, so it is still the better pick for lighting lenses and transparent covers where chemical exposure is not a factor.

Does PC-PBT need drying before molding?

Yes. Both the PC and PBT phases absorb moisture, and molding wet resin causes splay, silver streaks, and hydrolysis that weakens the PBT fraction. Dry at 120 °C for 3–4 hours and confirm a moisture level below 0.02% before processing to protect both appearance and mechanical strength.

What is the heat deflection temperature of PC-PBT?

Most unfilled PC-PBT grades reach an HDT of roughly 110–130 °C at 1.8 MPa, with the exact value set by the PC-to-PBT ratio. More PC content raises heat resistance; more PBT improves chemical resistance and flow. Glass-filled versions push the HDT higher for hotter under-hood positions.

How much does PC-PBT shrink during molding?

Expect about 0.6–1.2% shrinkage for unfilled grades. It is more uniform and predictable than semi-crystalline PBT alone, which helps large exterior panels hold their fit. Keep wall sections consistent and design with the specific grade's shrinkage data, since the polycarbonate and PBT phases pull in different directions.

Looking for a Reliable PC-PBT Injection Molding Partner?

Upload your drawings and note any fuel, oil, or grease exposure — we will recommend the right PC-PBT grade, quote your project, and include a free DFM analysis.

Shinzoft serves customers worldwide with custom PC-PBT injection molding solutions from prototype to mass production. See the full range on our materials page.

Get a Free Quote →
TYPE TO SEARCH

Tel:+86 0752-3336216
Email:Sales@shinzoft.com