LLDPE (Linear Low-Density Polyethylene) is a linear polyethylene with short-chain branching and a density of 0.915–0.935 g/cm³. It delivers higher tensile strength, tear resistance, and puncture resistance than LDPE while keeping much of its flexibility, which makes it ideal for thin-wall containers, lids, flexible parts, and toys. Shinzoft provides OEM/ODM LLDPE injection molding from DFM and tooling through validated mass production.
Short-chain branching instead of long-chain branching gives LLDPE a tensile strength of 15–25 MPa — roughly 1.5 to 2 times that of LDPE at similar density — so thin sections hold up under real load.
Notch and puncture resistance far exceed LDPE, which is why LLDPE dominates thin-wall lids, living hinges, and flexible parts that get pulled, pierced, or torn in service.
Excellent ESCR for a polyethylene, so LLDPE resists cracking under long-term stress in contact with detergents, oils, and chemicals — a common failure mode for LDPE and HDPE.
Modulus stays in the 250–450 MPa range, so parts remain flexible and soft-touch while withstanding impact and repeated flexing better than a softer LDPE grade would.
These values describe unfilled, general-purpose injection molding grades. LLDPE density and stiffness depend on comonomer type (butene, hexene, or octene), so a grade near 0.935 g/cm³ behaves noticeably stiffer than one near 0.915 g/cm³.
| Property | Typical Value | Notes |
|---|---|---|
| Density | 0.915–0.935 g/cm³ | Sits between LDPE and HDPE |
| Tensile Strength (Yield) | 15–25 MPa | Higher than LDPE at comparable density |
| Flexural Modulus | 250–450 MPa | Flexible yet tougher than LDPE |
| Elongation at Break | >600% | Very high ductility with strong tear resistance |
| Heat Deflection Temp (HDT, 1.8 MPa) | 45–60 °C | Slightly better heat resistance than LDPE |
| Melting Point | 120–130 °C | Higher than LDPE due to linear structure |
| Molding Shrinkage | 1.5–3.5 % | Moderate; watch flow-direction variation |
| Water Absorption | <0.01 % | Non-hygroscopic, no drying needed |
| Dielectric Strength | 18–25 kV/mm | Good insulation for flexible electrical parts |
| Parameter | Typical Range |
|---|---|
| Drying Temperature / Time | Not required (non-hygroscopic; keep pellets clean and dry) |
| Melt Temperature | 190–240 °C |
| Mold Temperature | 20–50 °C |
| Injection Pressure | 60–110 MPa |
| Holding Pressure | 35–65 MPa |
| Typical Cycle Time | 15–45 s (depends on wall thickness) |
LLDPE needs a somewhat higher melt temperature than LDPE because its linear structure is more viscous and less shear-thinning, but it delivers better melt strength and easier demolding as a result. That combination makes thin-wall and long-flow parts more forgiving than LDPE. Watch for flow-direction shrinkage differences on large flat lids, and add balanced cooling so the flatter, stiffer part does not twist on ejection.
LLDPE exists because LDPE could not keep up in thin sections. Against LDPE, it raises tensile strength, tear resistance, and ESCR while staying flexible, which lets designers reduce wall thickness and part weight. Against HDPE, LLDPE gives up some stiffness and chemical resistance but wins clearly on puncture toughness and stress crack resistance, and molds with better melt strength in long-flow parts. Against PP, LLDPE is softer, more flexible, and tougher at low temperature, while PP remains the choice for stiffness, heat resistance, and long-life living hinges.
Molecular structure. LDPE has long-chain branching, while LLDPE has a linear backbone with short-chain branches. That linear structure raises tensile strength, tear resistance, puncture resistance, and ESCR, so LLDPE holds up better in thin walls and long-flow parts while still molding as a flexible polyethylene.
Injection molded LLDPE walls can go down to roughly 0.8–1.2 mm depending on part size and flow length. LLDPE's better melt strength and toughness are what make those thin walls possible without tearing. Send us the geometry and we will confirm the minimum workable thickness during DFM review.
Yes, generally. LLDPE tolerates more flex cycles than LDPE before stress whitening or tearing appears, which makes it a good fit for snap lids and flexible closures. For very high cycle counts or hot environments, PP homopolymer still outperforms both and is the usual specification for long-life hinges.
Typically 190–240 °C, with mold temperature around 20–50 °C. LLDPE is more viscous than LDPE because of its linear structure, so it needs a bit more heat and slightly larger gates. In return it delivers better melt strength and easier demolding, which suits thin-wall and long-flow parts.
No. Like the rest of the polyethylene family, LLDPE is non-hygroscopic with water absorption below 0.01%, so it does not need drying. Keep pellets clean and dry during storage; only surface condensation from cold or damp storage needs a short low-temperature dry before molding.
Upload your drawings and receive a quote with a free DFM analysis covering thin-wall limits, gating, and cooling balance.
Shinzoft serves customers worldwide with custom LLDPE injection molding solutions, and you can review the full range on our materials page.
Get a Free Quote →