LCP (Liquid Crystal Polymer) Injection Molding Supplier & Manufacturer

Liquid crystal polymer (LCP) is a wholly aromatic thermoplastic whose rigid rod-like chains align in the melt, producing exceptional flow into walls as thin as 0.2 mm, near-zero flow-direction shrinkage (0.0–0.3%), and very low dielectric loss for high-frequency signals. Melting runs 280–330 °C with continuous service up to 200–240 °C. LCP serves micro connectors for phones and SIM sockets, 5G RF components, sensor bobbins, and miniature pump parts. Shinzoft delivers OEM/ODM LCP injection molding from DFM and tooling through validated mass production.

Key Properties of LCP for Injection Molding

Ultra-High Melt Flow

Because the molecular chains slide past one another in liquid crystalline order, LCP viscosity drops sharply under shear. That combination of low viscosity and high stiffness fills 0.2 mm walls over long flow lengths at moderate pressure.

Near-Zero Shrinkage

Flow-direction shrinkage runs 0.0–0.3%, giving LCP the tightest dimensional control of any common engineering resin. Shrinkage is also anisotropic, so parts differ between flow and cross-flow directions — a difference to design around, not ignore.

Low Dielectric Loss

LCP keeps a low, stable dielectric constant and dissipation factor well into the gigahertz range, and its low moisture uptake keeps those values from drifting. That suits high-frequency connectors, antenna modules, and RF substrates.

Heat & Chemical Resistance

With a 280–330 °C melting point, LCP handles continuous service at 200–240 °C and survives SMT reflow without distortion. It resists most solvents, fuels, and acids, and reaches UL94 V-0 without additives.

Technical Specifications of LCP

Values shown are typical for unfilled and 30% glass-filled LCP grades used in connectors and electronics.

PropertyTypical ValueNotes
Density1.35–1.40 g/cm³Unfilled; ~1.62 with 30% glass fiber
Tensile Strength150–200 MPaHighly direction-dependent, higher along flow
Flexural Modulus9,000–14,000 MPaStiff even in thin sections
Heat Deflection Temp (HDT, 1.8 MPa)200–240 °CWithstands lead-free reflow soldering
Melting Point / Tg280–330 °CDepends on the specific LCP chemistry
Molding Shrinkage0.0–0.3 % flow / 0.4–0.8 % crossAnisotropic; gate direction matters
Dielectric Constant (1 GHz)~3.0–3.3Low dissipation factor, stable with humidity

Applications of LCP Injection Molding

  • ✅ Micro Connectors: Phone board-to-board connectors, SIM and memory card sockets, and fine-pitch headers with sub-millimeter spacing.
  • ✅ 5G & High-Frequency Parts: Antenna modules, RF connector bodies, and waveguide components where low dielectric loss protects signal integrity.
  • ✅ Sensor Components: Sensor bobbins, housings, and carriers that hold position through reflow soldering and thermal cycling.
  • ✅ Bobbins & Coil Formers: Thin-wall winding bobbins and transformer or inductor formers needing heat resistance and tight wire-spacing tolerances.
  • ✅ Miniature Fluid Handling: Micro pump housings, valve bodies, and dosing components needing chemical resistance with precision fit.

LCP Injection Molding Process Parameters

ParameterTypical Range
Drying Temperature / Time150 °C / 3–4 h
Melt Temperature300–350 °C (high-temperature barrel)
Mold Temperature70–130 °C
Injection Pressure50–120 MPa
Injection SpeedHigh speed preferred
Typical Cycle Time8–25 s for thin-wall parts

LCP's own anisotropy creates most of the process risk. High shear aligns the molecular chains, which produces the low viscosity and low flow-direction shrinkage, but it also makes the melt shear-sensitive: excessive injection speed, abrupt gate restrictions, and sharp flow-path changes cause orientation build-up and defects such as delamination or splay. Weld lines are the other weak point, because chains aligned along two meeting flow fronts do not knit well, so their location and strength need review at the design stage. Barrels should be rated for the 300–350 °C window, and the material must be dried and kept dry, since moisture drives silver streaking and hydrolysis.

Design & Tooling Considerations for LCP

  • Plan for anisotropic shrinkage: Set gate location so the critical dimension runs in the flow direction, where shrinkage is 0.0–0.3%, and account for the higher cross-flow value in the same part.
  • Control weld lines: Keep weld lines out of load-bearing or sealing areas, or place them where the knit-line strength loss will not matter; balance the runner so they form predictably.
  • Gate and runner design: Use generous, short gates and avoid sharp corners or abrupt thickness changes that promote shear orientation near the gate.
  • Vent thoroughly: Thin walls and fast fill trap gas quickly; add deep, well-placed vents and check them for flash, since LCP's low viscosity flashes easily at loose shut-offs.
  • Thin-wall tooling accuracy: For 0.2 mm features, tool steel quality, core-pin support, and surface finish matter as much as the process; plan for high-precision EDM and tight parting-line control.

LCP vs Other Injection Molding Materials

LCP is chosen for flow and dimensional precision more than raw strength. When a part needs stiffness at 250 °C plus and full chemical resistance rather than ultra-thin walls, PEEK injection molding is the stronger option. Where an application needs transparency, flame retardancy, and lower cost but tolerates a lower flow ceiling, PEI (Polyetherimide) injection molding covers sterilization trays and electrical hardware. For engine-bay housings, LED reflectors, and structural connectors where toughness and cost matter more, PPA injection molding fits better.

Related Injection Molding Materials

  • PPA Injection Molding — high-temperature polyamide for connectors, LED reflectors, and under-hood housings with better toughness and lower cost.
  • PEEK Injection Molding — semi-crystalline resin with a 260 °C continuous rating and near-universal chemical resistance.
  • PEI Injection Molding — amber-transparent amorphous polymer with a 217 °C glass transition and inherent V-0 rating.

Why Choose Our Factory for LCP Injection Molding

  • ISO 9001 Certified Quality: Our Shenzhen headquarters and Huizhou factory run an ISO 9001 system with RoHS and REACH documentation plus dimensional reports on connector work.
  • 15+ Years of Experience: Founded in 2010, we have delivered more than 30 million molded parts to over 1,000 customers, including fine-pitch connector and thin-wall electronics work.
  • High-Temperature Barrel Capacity: More than 50 machines with barrels rated for 350 °C melts plus high-speed injection units suited to LCP's shear-sensitive flow.
  • Free DFM Analysis: We review gate location, weld-line placement, wall thickness, and anisotropic shrinkage before tooling, then verify cavity balance on the first trial.
  • No Minimum Order Quantity & Fast Lead Time: Prototype and production volumes use the same tooling, and most orders ship within 15 working days.

FAQs About LCP Injection Molding

What makes LCP different from ordinary engineering plastics?

LCP's molecular chains are rigid and rod-like, so they align in ordered domains in the melt rather than tangling like a normal polymer. That structure gives low viscosity even at high molecular weight, which is why LCP fills 0.2 mm walls and holds flow-direction shrinkage of just 0.0–0.3%.

Why is LCP shrinkage different in different directions?

Flow aligns the molecular chains, so the part shrinks very little along the flow direction (0.0–0.3%) but noticeably more across it (typically 0.4–0.8%). Design the gate so critical tolerances run in the flow direction, and expect the cross-flow figure to govern the other axis. Glass-filled grades reduce, but do not remove, the anisotropy.

How do you handle LCP's shear sensitivity during molding?

We keep injection speed high enough to fill thin walls but avoid the shear that causes delamination near gates, use generous gates and smooth transitions to limit orientation build-up, and verify venting so trapped gas does not burn the surface. Melt temperature stays in the 300–350 °C band with short residence times.

Are LCP weld lines a problem in molded parts?

Yes, weld lines are LCP's main mechanical weakness. Chains aligned along two meeting flow fronts do not knot together, so the joint reaches only a fraction of the base tensile strength. We balance runners and gates so weld lines land in low-stress zones rather than near latches, seals, or contacts.

Why is LCP used for 5G and high-frequency connectors?

LCP holds a low dielectric constant of roughly 3.0–3.3 and a low dissipation factor that stays stable from a few GHz into millimeter-wave bands, and its low moisture absorption keeps those values from drifting. That, plus 200–240 °C heat resistance for reflow soldering, suits antenna modules and fine-pitch RF connectors.

Looking for a Reliable LCP Injection Molding Partner?

Send us your drawings with your wall thickness, tolerance, and electrical requirements. You will get a quote and a free DFM analysis covering gate location, shrinkage, and weld-line placement.

Shinzoft serves customers worldwide with custom LCP injection molding solutions, from micro-connector tooling to repeat production. Explore our materials range for comparison.

Get a Free Quote →
TYPE TO SEARCH

Tel:+86 0752-3336216
Email:Sales@shinzoft.com