Start overmolding troubleshooting by identifying which material, interface, or feature failed and when the failure appeared. A layer that peels after chemical exposure needs a different investigation from flash caused by a misseated substrate. Increasing pressure to cure a short shot can also move the substrate or force material past the shutoff.