ABS-PC Alloy Injection Molding Supplier & Manufacturer

ABS-PC is a thermoplastic alloy that combines the easy flow, low cost, and good surface finish of ABS with the higher heat resistance, impact strength, and dimensional stability of polycarbonate. It keeps useful toughness from roughly −30 °C up to 100 °C plus, while molding faster and filling thinner walls than pure PC. Common uses include automotive interior trim, dashboard components, laptop and electronics housings, and appliance bodies. Shinzoft provides OEM/ODM ABS-PC injection molding from DFM and tooling through validated mass production.

Key Properties of ABS-PC for Injection Molding

Balanced Heat Resistance

With more PC in the blend, heat deflection temperatures reach about 90–125 °C at 1.8 MPa. That is well above unfilled ABS, so parts survive dashboard, under-dash, and near-lamp environments that plain ABS cannot handle.

High Impact Strength

Notched Izod values of 300–550 J/m give the alloy real ductility at room and low temperature. Drop-prone electronics housings and interior trim stay intact instead of snapping when bent or struck.

Good Processability

ABS-PC flows better than pure PC and molds at lower pressures, so it fills thin-wall housings and long-flow tools more easily. Cycle times stay competitive with ABS, which keeps part cost in check.

Dimensional Stability

Shrinkage of only 0.4–0.7% is lower and more predictable than ABS alone. Combined with low moisture uptake versus nylon or PBT, parts hold tight tolerances and stay flat across humidity changes.

Technical Specifications of ABS-PC

Values reflect general-purpose unfilled ABS-PC grades; both the heat rating and flow shift with the ABS-to-PC ratio, so confirm the exact grade for critical tolerances.

PropertyTypical ValueNotes
Density1.10–1.20 g/cm³Depends on PC content
Tensile Strength45–60 MPaDuctile, not brittle
Flexural Modulus2,000–2,600 MPaStiffer than pure ABS
Notched Izod Impact300–550 J/mStrong at low temperature
Heat Deflection Temp (HDT, 1.8 MPa)90–125 °CHigher with more PC content
Melting Point / Tg~260 °C / 110–130 °CProcess melt; PC glass transition
Molding Shrinkage0.4–0.7 %Lower than ABS alone
Dielectric Strength15–22 kV/mmSuitable for enclosures

Applications of ABS-PC Injection Molding

  • ✅ Automotive Interior Trim: dashboard panels, glove box doors, pillar trims, air vent housings, console components
  • ✅ Electronics Housings: laptop shells, monitor frames, router and set-top-box enclosures, battery covers
  • ✅ Power Tool Bodies: drill and sander casings, battery pack shells, grips that must survive drops and knocks
  • ✅ Appliance Enclosures: small appliance bodies, control panels, vacuum and kitchen equipment covers
  • ✅ Medical & Lab Equipment: non-patient-contact housings, instrument shells where heat and impact resistance matter
  • ✅ EMI/RFI Shielded Parts: platable grades for conductive coatings on communication and computing hardware

ABS-PC Injection Molding Process Parameters

ParameterTypical Range
Drying Temperature / Time80–90 °C / 2–4 h
Melt Temperature230–280 °C
Mold Temperature60–100 °C
Injection Pressure60–110 MPa
Typical Cycle Time25–55 s (wall-thickness dependent)

ABS-PC is moisture sensitive because of the PC phase, so a proper 80–90 °C dry cycle is required to prevent splay, silver streaks, and hydrolysis that weakens the part. Keep melt temperatures below about 280 °C; overheating darkens the resin and drops impact strength. Mold temperature matters more than with ABS — run 70–100 °C for glossy, low-stress surfaces, and lower it only when surface finish is not critical, since cold tools leave a dull or blemished finish.

Design & Tooling Considerations for ABS-PC

  • Shrinkage planning: design around 0.4–0.7% and keep walls uniform. Low, stable shrinkage makes the alloy a good choice for tight-tolerance snap-fit and living-hinge-adjacent parts.
  • Mold temperature for gloss: budget for hotter mold water (70–100 °C). Cold molds produce a poor surface, so plan tooling cooling accordingly rather than treating it like ABS.
  • Gate design: use full-round or trapezoidal runners and a gate that avoids jetting. A fan or submarine gate works well on thin-wall housings to limit stress marks.
  • Venting: vent cavities adequately; trapped gas shows as burns on large flat areas such as laptop lids and dashboard skins.
  • Chemical exposure: ABS-PC resists many oils and cleaners but is attacked by strong solvents and some aromatics. Verify specific contact before specifying it for fuel-adjacent parts — PC-PBT may be the better pick there.

ABS-PC vs Other Injection Molding Materials

Against plain ABS, the alloy adds heat resistance, impact strength, and dimensional stability at the cost of some flow and price — worthwhile whenever a part sees heat or drops. Compared with pure PC, ABS-PC flows and fills far better and costs less, trading a little peak clarity and toughness; it is the practical default for most opaque, high-impact housings. Where parts contact fuels, oils, or greases, PC-PBT alloy resists those chemicals that ABS-PC does not.

Related Injection Molding Materials

Why Choose Our Factory for ABS-PC Injection Molding

  • ISO 9001 Certified Quality: controlled drying, melt-temperature monitoring, and RoHS/REACH-compliant material handling for every production lot.
  • 15+ Years of Experience: established in 2010, we have produced 30M+ parts for 1,000+ customers across automotive, electronics, and consumer goods.
  • Free DFM Analysis: alloy grades need hotter mold temperatures and careful gate placement, so we verify shrinkage, fill, and cooling before cutting steel.
  • Fast Lead Time & No MOQ: 50+ machines across our Shenzhen and Huizhou plants deliver most orders within 15 working days, with no minimum order quantity.

FAQs About ABS-PC Injection Molding

What is ABS-PC alloy used for?

ABS-PC is used where a part needs better heat and impact resistance than ABS but easier molding than pure PC. Typical parts include automotive interior trim and dashboards, laptop and electronics housings, power tool bodies, and appliance enclosures. It is the common default for opaque, drop-resistant, moderately heat-exposed plastic parts.

Is ABS-PC better than ABS for electronics housings?

For most housings, yes. ABS-PC stays tough at lower temperatures, resists warping near heat sources, and holds tighter tolerances thanks to its lower shrinkage. Plain ABS costs less and flows slightly better, so it remains valid for low-stress, room-temperature covers where budget is the priority.

Does ABS-PC need drying before molding?

Yes. The PC phase absorbs moisture, and molding wet resin causes splay, silver streaks, and hydrolysis that cuts impact strength. Dry at 80–90 °C for 2–4 hours and confirm a low moisture level before processing to keep both appearance and toughness intact.

What is the heat deflection temperature of ABS-PC?

Most unfilled ABS-PC grades reach an HDT of about 90–125 °C at 1.8 MPa, set by the ABS-to-PC ratio. More PC content raises heat resistance toward 125 °C; more ABS improves flow and lowers cost. Glass-filled versions push the HDT higher for hotter positions.

How much does ABS-PC shrink during molding?

Expect about 0.4–0.7% shrinkage for unfilled grades, lower and more predictable than ABS alone. That tight, stable shrinkage is why the alloy suits snap-fit and tight-tolerance housings. Keep wall sections consistent and design with the specific grade's shrinkage data.

Looking for a Reliable ABS-PC Injection Molding Partner?

Upload your drawings and note any heat or drop requirements — we will recommend the right ABS-PC grade, quote your project, and include a free DFM analysis.

Shinzoft serves customers worldwide with custom ABS-PC injection molding solutions from prototype to mass production. See the full range on our materials page.

Get a Free Quote →
TYPE TO SEARCH

Tel:+86 0752-3336216
Email:Sales@shinzoft.com